Capabilities of Nd:YVO4 Crystal: 

Nd dopant:0.27%, 0.3%, 0.4%, 0.5%, 0.7%, 1.0%, 2.0%, 3.0%
Width x Height:1x1 ~ 16x16mm
Length:0.02 ~ 20mm


Specifications of Nd:YVO4 Crystal:

Orientation:a-cut( ± 0.5° )
Dimensional Tolerance:+/-0.1mm
Wavefront Distortion:<λ/8 at 633nm
Surface Quality:20/10
Parallelism:< 10 arc seconds
Perpendicularity:< 5 arc minutes
Surface Flatness:<λ/10 at 632.8nm
Clear Aperture:Central 95%
Chamfer:0.15x45°
Coating:1.AR@1064nm R<0.1%
2.AR@1064nm R< 0.1% & HT@808nm T>95% 
3.HR@1064nm R>99.8% & HR@532nm R>99% & HT@808nm T>95%


Properties of Nd:YVO4 Crystal: 

Atomic Density~1.37x1020 atoms/cm2
Crystal StructureZircon Tetragonal, space group D4h, a=b=7.12, c=6.29
Density4.22 g/cm3
Mohs HardnessGlass-like, ~5
Thermal Expansion Coefficientaa=4.43x10-6/K, ac=11.37x10-6/K
Thermal Conductivity Coefficient||C: 5.23 W/m/K; ^C: 5.10 W/m/K


Lasing Wavelengths914nm, 1064 nm, 1342 nm
Crystal Classpositive uniaxial, no=na=nb ne=nc
no=1.9573, ne=2.1652, @ 1064nm
no=1.9721, ne=2.1858, @ 808nm
no=2.0210, ne=2.2560, @ 532nm
Thermal Optical Coefficientdna/dT=8.5x10-6/K, dnc/dT=3.0x10-6/K
Stimulated Emission Cross-Section25.0x10-19 cm2 , @1064 nm
Fluorescent Lifetime90μs(about 50μs for 2 atm% Nd doped) @ 808 nm
Absorption Coefficient31.4 cm-1 @ 808 nm
Absorption Length0.32 mm @ 808 nm
Intrinsic LossLess 0.1% cm-1 , @1064 nm
Gain Bandwidth0.96 nm (257 GHz) @ 1064 nm
Polarized Laser Emissionp parallel to optic axis (c-axis)
Diode Pumped Optical to Optical Efficiency> 60%

Sellmeier Equation (for pure YVO4 crystals)
no2=3.77834+0.069736/(λ2 - 0.04724) - 0.0108133λ2
no2=4.59905+0.110534/(λ2 - 0.04813) - 0.0122676λ2